Laser beam microstructuring of magnesium sheets made of ME20 – Potentials for the in-mould assembly of plastic/magnesium hybrid joints


Peer-reviewed papers

Authors: Prof. Dr.-Ing. Christian Hopmann, Dipl.-Wirt.Ing. Christoph Engelmann, M. Sc. Simon Wurzbacher

Practical aspects, above all the selection of components, are described in this last part of the total of three articles about the absorber-free laser beam ...
Pages: 182 - 187
Ausgabe 3-4 (2019) Jahrgang 13 Page 182
Ausgabe 3-4 (2019) Jahrgang 13 Page 183
Ausgabe 3-4 (2019) Jahrgang 13 Page 184
Ausgabe 3-4 (2019) Jahrgang 13 Page 185
Ausgabe 3-4 (2019) Jahrgang 13 Page 186
Ausgabe 3-4 (2019) Jahrgang 13 Page 187

This article appeared in issue 3 (2019).

Issue 3-4 (2019) Volume 13
Joining Plastics
Issue 3-4 (2019) Volume 13
› learn more
An active subscription enables you to download articles or entire issues as PDF-files. If you already are a subscriber, please login. More information about the subscription

More content

- Advertisement -
- Advertisement -
- Advertisement -